- Plates, Sheets, Film, Foil And Strip, Of Non-cellular Polymers Of Ethylene, Not Reinforced, Laminated, Supported Or Similarly Combined With Other Materials, Without Backing, Unworked Or Merely Surface-worked Or Merely Cut Into Squares Or Rectangles (excl. Self-adhesive Products, And Floor, Wall And Ceiling Coverings Of Heading 3918)
Bopp thermal lamination film
Product Images
Product Property
Product Status : | New |
Sample Available : | yes |
Shipment Terms : | fob |
Payment Mode : |
T/T,WesternUnion |
Description
Bopp thermal lamination film
SPECIFICATION & PARAMETER
MATERIAL
Surface layer: BOPP
glue layer: EVA adhesive
SPECIFICATION
Thickness:
Glossy : | 18mic (12+6), 20mic (12+8), 22mic (12+10), 23mic (15+8), |
24mic (12+12) , 25mic (15+10), 27mic (15+12), 30mic(18+12) | |
Matte: | 18mic (12+6), 20mic (12+8), 22mic (12+10), 23mic (15+8), |
24mic (12+12) , 25mic (15+10), 27mic (15+12), 30mic(18+12) |
Width: 250~1880mm
Length: 100~4000M
Paper core: 25.4mm (1 inch), 58mm(2.25inches), 76mm(3 inches)
Bonding: less than 2
Process Parameter:
- ·Equipment for thermal film: dry and wet film laminator
- ·lamination temperature: 95~105℃
- ·Roller pressure: 10-20Mpa
- ·Speed: 8-20 m/min
Directions for using BOPP thermal laminating film:
1. | Normal process temperature is 90℃-105℃, roller pressure and temperature vary with different types of paper, ink and machines. |
2. | When using the film for the first time or do other treatment, try a small volume before mass laminating. |
3. | Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder. |
4. | Make sure put the material in a low-temperature, dry place. |