Silicone Rubber for Spin Casting
Product Images
Product Property
Product Status : | New |
Sample Available : | yes |
Shipment Terms : | fob,cfr,cif,Negotiable |
Payment Mode : |
T/T |
Description
Wide range of specially formulated silicone rubbers to meet different demands for spin casting of low-melt zinc alloy and tin-lead alloy.
Available size: 9", 12", 14", 16".
PA, pin color,
Application: Suitable for zinc alloy spin casting.
Vulcanizing temperature: 165 degree C
Vulcanizing time: 60mins.
Shore hardness after vulcanizing: 75
Tear-resistant strength: 98Mpa
Elongation: 32%
Highest heat-resistance (10 secs): 750 degree C
GA, Green color,
Application: Suitable for tin-lead alloy spin casting of flat parts
Vulcanizing temperature: 150-165 degree C
Vulcanizing time: 60 mins.
Shore hardness after vulcanizing: 65
Tear-resistant strength: 80Mpa
Elongation: 58%
Highest heat-resistance (10 secs): 500 degree C
BA, Blue color,
Application: Suitable for tin-lead alloy spin casting of miniature figurines, photo frame etc.
Vulcanizing temperature: 165 degree C
Vulcanizing time: 60 mins.
Shore hardness after vulcanizing: 70
Tear-resistant strength: 95Mpa
Elongation: 72%
Highest heat-resistance (10 secs): 500 degree C
YB, yellor color,
Specially developed cheaper silicon rubber, mainly used to reduce cost, half or 1/3 thick of the mold, not directly contact alloy.
Available size: 9", 12", 14", 16".
PA, pin color,
Application: Suitable for zinc alloy spin casting.
Vulcanizing temperature: 165 degree C
Vulcanizing time: 60mins.
Shore hardness after vulcanizing: 75
Tear-resistant strength: 98Mpa
Elongation: 32%
Highest heat-resistance (10 secs): 750 degree C
GA, Green color,
Application: Suitable for tin-lead alloy spin casting of flat parts
Vulcanizing temperature: 150-165 degree C
Vulcanizing time: 60 mins.
Shore hardness after vulcanizing: 65
Tear-resistant strength: 80Mpa
Elongation: 58%
Highest heat-resistance (10 secs): 500 degree C
BA, Blue color,
Application: Suitable for tin-lead alloy spin casting of miniature figurines, photo frame etc.
Vulcanizing temperature: 165 degree C
Vulcanizing time: 60 mins.
Shore hardness after vulcanizing: 70
Tear-resistant strength: 95Mpa
Elongation: 72%
Highest heat-resistance (10 secs): 500 degree C
YB, yellor color,
Specially developed cheaper silicon rubber, mainly used to reduce cost, half or 1/3 thick of the mold, not directly contact alloy.